PolyOne Bergamid™ A70 G25 H U-SO Polyamide 66 (Nylon 66)

Category Polymer , Thermoplastic , Nylon , Nylon 66
Manufacturer PolyOne Corporation
Trade Name Bergamid™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Bergamid™ A70 G25 H U-SO Polyamide 66 (Nylon 66).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Density 1.38 g/cc
0.0499 lb/in³
±0.02 g/cm³; DIN 53479
Ash 25 %
25 %
ISO 3451
Mechanical Properties Metric English Comments
Tensile Strength at Break 160 MPa

@Temperature 23.0 °C
23200 psi

@Temperature 73.4 °F
ISO 527-2/5
Elongation at Break 3.0 %

@Temperature 23.0 °C
3.0 %

@Temperature 73.4 °F
ISO 527-2/5
Tensile Modulus 8.50 GPa

@Temperature 23.0 °C
1230 ksi

@Temperature 73.4 °F
ISO 527-2/1
Charpy Impact Unnotched 6.00 J/cm²

@Temperature -30.0 °C
28.6 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
6.50 J/cm²

@Temperature 23.0 °C
30.9 ft-lb/in²

@Temperature 73.4 °F
Type 1; ISO 179/1eA
Charpy Impact, Notched 0.900 J/cm²

@Temperature -30.0 °C
4.28 ft-lb/in²

@Temperature -22.0 °F
ISO 179/1eA
1.20 J/cm²

@Temperature 23.0 °C
5.71 ft-lb/in²

@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 261 °C
502 °F
ISO 3146
Maximum Service Temperature, Air 120 °C
248 °F
Continuous (GTP 50% Tensile); IEC 60216
220 °C
428 °F
Short Time; IEC 60216
Deflection Temperature at 0.46 MPa (66 psi) 250 °C
482 °F
Unannealed; ISO 75-2/B
Flammability, UL94 V-0

@Thickness 3.00 mm
V-0

@Thickness 0.118 in
ALL; Internal Method
Glow Wire Test 960 °C

@Thickness 3.00 mm
1760 °F

@Thickness 0.118 in
0.8 mm wire; Ignition Temperature; IEC 60695-2-13
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 ohm-cm
1.00e+15 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Dielectric Constant 3.5

@Frequency 1.00e+6 Hz
3.5

@Frequency 1.00e+6 Hz
IEC 60250
Dielectric Strength 80.0 kV/mm
2030 kV/in
IEC 60243-1
Dissipation Factor 0.015

@Frequency 1.00e+6 Hz
0.015

@Frequency 1.00e+6 Hz
IEC 60250
Comparative Tracking Index 400 V
400 V
Solution A; IEC 60112
Descriptive Properties Value Comments
Additive Heat Stabilizer
Features Flame Retardant
Halogen Free
Heat Stabilized
Filler / Reinforcement Glass Fiber Reinforcement, 25% Filler by Weight
Forms Pellets
Generic Material Nylon 66
Generic Name Polyamide 66 (Nylon 66)
Regional Availability Africa & Middle East
Asia Pacific
Europe
RoHS Compliance RoHS Compliant