Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne™ Corporation
Physical Properties Metric English Comments
Specific Gravity 1.58 g/cc
1.58 g/cc
ASTM D792
Water Absorption 0.25 %

@Thickness 3.17 mm
0.25 %

@Thickness 0.125 in
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm
0.0020 - 0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 257 MPa
37300 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 1.0 - 3.0 %
1.0 - 3.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 17.2 GPa
2500 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 310 MPa
45000 psi
ASTM D790
Flexural Modulus 13.8 GPa
2000 ksi
ASTM D790
Izod Impact, Notched 1.33 J/cm
2.50 ft-lb/in
Method A, Injection Molded, 0.125 in bars, 73°F; ASTM D648
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 302 °C
575 °F
Unannealed, 0.125 in bars; ASTM D648
Processing Properties Metric English Comments
Melt Temperature 321 - 349 °C
610 - 660 °F
Molding
Descriptive Properties Value Comments
Processing Method Injection Molding