Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Edgetek® AS-10GF/000 NATURAL Acrylonitrile Butadiene Styrene (ABS)

Category Polymer , Thermoplastic , ABS Polymer
Manufacturer PolyOne Corporation
Trade Name Edgetek®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® AS-10GF/000 NATURAL Acrylonitrile Butadiene Styrene (ABS).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.11 g/cc
1.11 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm
0.0020 - 0.0040 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0075 - 0.010 cm/cm
0.0075 - 0.010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 59.3 MPa
8600 psi
5.1 mm/min; ASTM D638
Elongation at Break 2.0 - 3.0 %
2.0 - 3.0 %
ASTM D638
Tensile Modulus 4.12 GPa
598 ksi
5.1 mm/min; ASTM D638
Flexural Strength 93.8 MPa
13600 psi
1.3 mm/min; ASTM D790
Flexural Modulus 3.79 GPa
550 ksi
1.3 mm/min; ASTM D790
Izod Impact, Notched 0.750 J/cm
1.41 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 100 °C
212 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 91.0 °C
196 °F
Unannealed; ASTM D648
Descriptive Properties Value Comments
Features Amorphous
Good Moldability
Good Toughness
Filler / Reinforcement Glass Fiber Reinforcement, 10% Filler by Weight
Forms Pellets
Generic Material ABS
Generic Name Acrylonitrile Butadiene Styrene (ABS)
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Uses Appliances
Automotive Applications
Consumer Applications
General Purpose
Industrial Applications
Structural Parts
Users viewing this material also viewed the following: