Material Notes:
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.18 g/cc
1.18 g/cc
ASTM D792
Water Absorption 0.050 %
0.050 %
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0030 cm/cm
0.0020 - 0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 107
107
ASTM D785
Tensile Strength at Break 70.7 MPa
10300 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 6.0 %
6.0 %
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 117 MPa
17000 psi
ASTM D790
Flexural Modulus 3.45 GPa
500 ksi
ASTM D790
Izod Impact, Notched 0.590 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.11 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
0.610 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.14 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 36.0 µm/m-°C
20.0 µin/in-°F
ASTM D696
Thermal Conductivity 0.200 W/m-K
1.39 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 98.9 °C

@Thickness 3.18 mm
210 °F

@Thickness 0.125 in
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 91.1 °C

@Thickness 3.18 mm
196 °F

@Thickness 0.125 in
Annealed; ASTM D648
Flammability, UL94 HB
HB
UL 94
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 221 - 249 °C
430 - 480 °F
Mold Temperature 65.0 - 85.0 °C
149 - 185 °F
Drying Temperature 80.0 - 85.0 °C
176 - 185 °F
Dry Time 2.00 hour
2.00 hour
Descriptive Properties Value Comments
Filler / Reinforcement Glass Fiber Reinforcement, 20% Filler by Weight
Forms Pellets
Generic Material ABS
Generic Name Acrylonitrile Butadiene Styrene (ABS)
Regional Availability Africa & Middle East