PolyOne Edgetek® ET3500-5001 colored Acrylonitrile Styrene Acrylate + PC (ASA+PC)

Category Polymer , Thermoplastic , ASA Polymer , Polycarbonate (PC)
Manufacturer PolyOne Corporation
Trade Name Edgetek®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® ET3500-5001 colored Acrylonitrile Styrene Acrylate + PC (ASA+PC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Edgetek™ Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.Information provided by PolyOne
Physical Properties Metric English Comments
Density 1.15 g/cc

@Temperature 23.0 °C
0.0415 lb/in³

@Temperature 73.4 °F
ISO 1183
Water Absorption 0.15 %
0.15 %
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0010 - 0.0040 cm/cm
0.0010 - 0.0040 in/in
ASTM D955
Melt Index of Compound >= 22 g/10 min

@Load 2.16 kg,
Temperature 260 °C
>= 22 g/10 min

@Load 4.76 lb,
Temperature 500 °F
cm³/10min; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 60.0 MPa
8700 psi
ISO 527-2
Elongation at Yield 5.0 %
5.0 %
ISO 527-2
Tensile Modulus 2.50 GPa

@Thickness 4.00 mm,
Temperature 23.0 °C
363 ksi

@Thickness 0.157 in,
Temperature 73.4 °F
Injection Molded; ISO 527-2/1
Charpy Impact Unnotched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
Injection Molded; ISO 179
Charpy Impact, Notched 1.00 J/cm²

@Temperature -30.0 °C
4.76 ft-lb/in²

@Temperature -22.0 °F
ISO 179
4.00 J/cm²

@Temperature 23.0 °C
19.0 ft-lb/in²

@Temperature 73.4 °F
Injection Molded; ISO 179
Thermal Properties Metric English Comments
Vicat Softening Point 117 °C
243 °F
ISO 306/B50
129 °C
264 °F
ISO 306/A50
Flammability, UL94 HB
HB
UL 94
Electrical Properties Metric English Comments
Volume Resistivity >= 1.00e+15 ohm-cm
>= 1.00e+15 ohm-cm
ASTM D257
Surface Resistance >= 1.00e+14 ohm
>= 1.00e+14 ohm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 255 - 285 °C
491 - 545 °F
Mold Temperature 82.0 - 110 °C
180 - 230 °F
Drying Temperature 120 °C
248 °F
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Descriptive Properties Value Comments
Features Low Warpage
Forms Pellets
Generic Material ASA+PC
Generic Name Acrylonitrile Styrene Acrylate + PC (ASA+PC)
Regional Availability Europe
RoHS Compliance RoHS Compliant
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved