Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Edgetek® ET5200-0018 UV RS Desert Sage Polypropylene Homopolymer (PP Homopolymer)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer PolyOne Corporation
Trade Name Edgetek®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® ET5200-0018 UV RS Desert Sage Polypropylene Homopolymer (PP Homopolymer).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0010 - 0.0040 cm/cm
0.0010 - 0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.4 MPa
6000 psi
Type I, 51 mm/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
Type I, 51 mm/min; ASTM D638
Flexural Strength 60.0 MPa
8700 psi
ASTM D790
Flexural Modulus 2.80 GPa
406 ksi
ASTM D790
Izod Impact, Notched 0.270 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.506 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 150 °C

@Thickness 3.18 mm
302 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Descriptive Properties Value Comments
Appearance Natural Color
Features General Purpose
Homopolymer
Filler / Reinforcement Glass Fiber Reinforcement
Unspecified FillerReinfor., 20% Filler by Weight
Forms Pellets
Generic Material PP Homopolymer
Generic Name Polypropylene Homopolymer (PP Homopolymer)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Automotive Applications
Construction Applications
Consumer Applications
General Purpose
Industrial Applications
Copyright © lookpolymers.com All Rights Reserved