PolyOne Edgetek® MP-1000 Modified PPO - Unreinforced  (discontinued **)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® MP-1000 Modified PPO - Unreinforced  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by PolyOne.
Physical Properties Metric English Comments
Density 1.06 g/cc
0.0383 lb/in³
ASTM D792
Water Absorption 0.060 %
0.060 %
24 hrs. ASTM D570
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm

@Thickness 3.17 mm
0.0050 - 0.0070 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 119
119
ASTM D785
Tensile Strength, Ultimate 66.0 MPa
9570 psi
ASTM D638
Flexural Yield Strength 93.0 MPa
13500 psi
ASTM D790
Flexural Modulus 2.48 GPa
360 ksi
ASTM D790
Thermal Properties Metric English Comments
CTE, linear 59.4 µm/m-°C

@Temperature 20.0 °C
33.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 137 °C
279 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 129 °C
264 °F
ASTM D648
Flammability, UL94 HB
HB