Material Notes:
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.13 g/cc
1.13 g/cc
ASTM D792
Water Absorption 0.30 %
0.30 %
@ 24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.0050 - 0.0060 cm/cm

@Thickness 3.18 mm
0.0050 - 0.0060 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 82.7 MPa
12000 psi
5.1 mm/min; ASTM D638
Elongation at Break 5.0 %
5.0 %
ASTM D638
Tensile Modulus 4.14 GPa
600 ksi
5.1 mm/min; ASTM D638
Flexural Strength 131 MPa
19000 psi
1.3 mm/min; ASTM D790
Flexural Modulus 3.45 GPa
500 ksi
1.3 mm/min; ASTM D790
Izod Impact, Notched 0.430 J/cm
0.806 ft-lb/in
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 200 °C
392 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 175 °C
347 °F
Unannealed; ASTM D648
Descriptive Properties Value Comments
Features Good Chemical Resistance
Good Stability
Low to No Water Absorption
Semi Crystalline
Filler / Reinforcement Glass Fiber Reinforcement, 10% Filler by Weight
Forms Pellets
Generic Material Nylon 612
Generic Name Polyamide 612 (Nylon 612)
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Uses Aerospace Applications
Appliance Components
Appliances
Automotive Applications
Electrical/Electronic Applications
Housings
Industrial Applications
Marine Applications
Sporting Goods
Copyright © lookpolymers.com All Rights Reserved