PolyOne Edgetek® PE-25CF/000 High Density Polyethylene (HDPE), Carbon Fiber Reinforced  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® PE-25CF/000 High Density Polyethylene (HDPE), Carbon Fiber Reinforced  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.08 g/cc
1.08 g/cc
ASTM D792
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm
0.0010 - 0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 53.8 MPa
7800 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 4.14 GPa
600 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Izod Impact, Notched 0.598 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.12 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Processing Properties Metric English Comments
Melt Temperature 204 - 221 °C
400 - 430 °F
Molding
Mold Temperature 26.7 - 54.4 °C
80.0 - 130 °F
Descriptive Properties Value Comments
Product Form Pellets