PolyOne Edgetek® PE-40MC/000 High Density Polyethylene (HDPE)  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® PE-40MC/000 High Density Polyethylene (HDPE)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Mica FilledInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.304 g/cc
1.304 g/cc
ASTM D792
Water Absorption 0.010 %

@Thickness 3.17 mm
0.010 %

@Thickness 0.125 in
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.0060 - 0.0070 cm/cm
0.0060 - 0.0070 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 34.5 MPa
5000 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 7.0 %
7.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 1.72 GPa
250 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 34.5 MPa
5000 psi
ASTM D790
Flexural Modulus 1.72 GPa
250 ksi
ASTM D790
Izod Impact, Notched 0.961 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.80 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256