PolyOne Edgetek® PF-10GF/000 Polysulfone, Glass Filled  (discontinued **)

Category Polymer , Thermoplastic , Polysulfone (PSU)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® PF-10GF/000 Polysulfone, Glass Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.30 g/cc
1.30 g/cc
ASTM D792
Water Absorption 0.20 %

@Thickness 3.17 mm
0.20 %

@Thickness 0.125 in
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.0040 - 0.0050 cm/cm
0.0040 - 0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 82.7 MPa
12000 psi
Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638
Elongation at Break 1.0 - 3.0 %
1.0 - 3.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 5.17 GPa
750 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 103 MPa
15000 psi
ASTM D790
Flexural Modulus 5.17 GPa
750 ksi
ASTM D790
Izod Impact, Notched 0.534 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.00 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 177 °C
350 °F
Unannealed; ASTM D648
Processing Properties Metric English Comments
Melt Temperature 343 - 382 °C
650 - 720 °F
Molding