PolyOne Edgetek® PF-30GF/000 Polysulfone, Glass Filled  (discontinued **)

Category Polymer , Thermoplastic , Polysulfone (PSU)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® PF-30GF/000 Polysulfone, Glass Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.46 g/cc
1.46 g/cc
ASTM D792
Water Absorption 0.20 %

@Thickness 3.17 mm
0.20 %

@Thickness 0.125 in
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.0020 - 0.0030 cm/cm
0.0020 - 0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 121 MPa
17500 psi
Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638
Elongation at Break 3.0 - 4.0 %
3.0 - 4.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 8.96 GPa
1300 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 165 MPa
24000 psi
ASTM D790
Flexural Modulus 7.58 GPa
1100 ksi
ASTM D790
Izod Impact, Notched 0.747 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.40 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 182 °C
360 °F
Unannealed; ASTM D648
Processing Properties Metric English Comments
Melt Temperature 332 - 371 °C
630 - 700 °F
Molding