PolyOne Edgetek® QT020GFS/000 FR NATURAL - OBSOLETE Syndiotactic Polystyrene (SPS)

Category Polymer , Thermoplastic , Polystyrene (PS) , Syndiotactic Polystyrene (SPS)
Manufacturer PolyOne Corporation
Trade Name Edgetek®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® QT020GFS/000 FR NATURAL - OBSOLETE Syndiotactic Polystyrene (SPS).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ISO 1183
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cm
0.0030 - 0.0050 in/in
ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 120 MPa
17400 psi
Type I, 5.0 mm/min; ISO 527
Elongation at Break 1.3 %
1.3 %
Type I, 5.0 mm/min; ISO 527
Tensile Modulus 9.00 GPa
1310 ksi
Type I, 5.0 mm/min; ISO 527
Flexural Strength 170 MPa
24700 psi
ISO 178
Flexural Modulus 9.50 GPa
1380 ksi
ISO 178
Charpy Impact Unnotched 3.40 J/cm²
16.2 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.550 J/cm²
2.62 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 230 °C

@Thickness 3.18 mm
446 °F

@Thickness 0.125 in
Unannealed; ISO 75-2/A
Flammability, UL94 HB
HB
UL 94
Processing Properties Metric English Comments
Melt Temperature 270 - 320 °C
518 - 608 °F
Mold Temperature 80.0 - 150 °C
176 - 302 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 2.00 hour
2.00 hour
Descriptive Properties Value Comments
Appearance Natural Color
Filler / Reinforcement Glass Fiber Reinforcement
Forms Pellets
Generic Material SPS
Generic Name Syndiotactic Polystyrene (SPS)
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America