PolyOne Edgetek® UR2-40CF/000 BLACK Polyurethane, Unspecified (PUR, Unspecified)

Category Polymer , Thermoplastic , Polyurethane, TP
Manufacturer PolyOne Corporation
Trade Name Edgetek®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® UR2-40CF/000 BLACK Polyurethane, Unspecified (PUR, Unspecified).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Linear Mold Shrinkage, Transverse 0.00090 - 0.0030 cm/cm
0.00090 - 0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 98.6 MPa
14300 psi
ASTM D638
Tensile Strength, Yield 103 MPa
14900 psi
ASTM D638
Elongation at Break 7.0 - 11 %
7.0 - 11 %
ASTM D638
Tensile Modulus 9.31 GPa
1350 ksi
5.1 mm/min; ASTM D638
Flexural Strength 131 MPa
19000 psi
1.3 mm/min; ASTM D790
Flexural Modulus 7.93 GPa
1150 ksi
1.3 mm/min; ASTM D790
Izod Impact, Notched 2.70 J/cm
5.06 ft-lb/in
Injection Molded; ASTM D256
Electrical Properties Metric English Comments
Volume Resistivity 100 - 10000 ohm-cm
100 - 10000 ohm-cm
ASTM D257
Surface Resistance 100 - 10000 ohm
100 - 10000 ohm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 216 - 238 °C
421 - 460 °F
Descriptive Properties Value Comments
Features Balanced Stiffness/Toughness
Electrically Conductive
Filler / Reinforcement Carbon Fiber Reinforcement, 40% Filler by Weight
Forms Pellets
Generic Material PUR, Unspecified
Generic Name Polyurethane, Unspecified (PUR, Unspecified)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Consumer Applications
Industrial Applications
Medical/Healthcare Applications
Users viewing this material also viewed the following: