Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Edgetek® X PS-154200101 WHITE Polybutylene Terephthalate (PBT)

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer PolyOne Corporation
Trade Name Edgetek®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® X PS-154200101 WHITE Polybutylene Terephthalate (PBT).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.48 g/cc
1.48 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 - 0.0060 cm/cm

@Thickness 3.18 mm
0.0030 - 0.0060 in/in

@Thickness 0.125 in
ASTM D955
Linear Mold Shrinkage, Transverse 0.013 - 0.022 cm/cm

@Thickness 3.18 mm
0.013 - 0.022 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 82.7 MPa
12000 psi
5.1 mm/min; ASTM D638
Elongation at Break 3.0 - 5.0 %
3.0 - 5.0 %
ASTM D638
Tensile Modulus 6.89 GPa
999 ksi
5.1 mm/min; ASTM D638
Flexural Strength 134 MPa
19400 psi
1.3 mm/min; ASTM D790
Flexural Modulus 6.62 GPa
960 ksi
1.3 mm/min; ASTM D790
Izod Impact, Notched 0.800 J/cm
1.50 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 245 °C
473 °F
Unannealed; ASTM D648
Descriptive Properties Value Comments
Features Good Chemical Resistance
High Heat Resistance
Impact Modified
Semi Crystalline
Filler / Reinforcement Glass Fiber Reinforcement, 30% Filler by Weight
Forms Pellets
Generic Material PBT
Generic Name Polybutylene Terephthalate (PBT)
Regional Availability North America
South America
Uses Appliance Components
Appliances
Automotive Applications
Consumer Applications
Housings
Industrial Applications
Sporting Goods
Structural Parts
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved