PolyOne Elastamax™ HTE 1104 Styrene Butadiene Block Copolymer (SBC)  (discontinued **)

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene-Butadiene Copolymer, SBC
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Elastamax™ HTE 1104 Styrene Butadiene Block Copolymer (SBC)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in accordance with accepted test methods. All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21 for use in the packaging of food. The listings cover many uses and restrictions may apply depending on the application. For More Information contact PolyOne.
Physical Properties Metric English Comments
Specific Gravity 0.928 g/cc
0.928 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
ASTM D2240
Tensile Strength at Break 9.10 MPa
1320 psi
510 mm/min; ASTM D412A
Tensile Strength, Yield 1.72 MPa

@Strain 100 %
249 psi

@Strain 100 %
510 mm/min; ASTM D412A
3.14 MPa

@Strain 300 %
455 psi

@Strain 300 %
510 mm/min; ASTM D412A
Elongation at Break 1000 %
1000 %
510 mm/min; ASTM D412A
Tear Strength 29.8 kN/m
170 pli
Die C, 510 mm/min; ASTM D624
Compression Set 16 %

@Temperature 23.0 °C,
Time 79200 sec
16 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395B
Descriptive Properties Value Comments
Agency Ratings FDA Food Contact, Unspecified Rating
Features Food Contact Acceptable
General Purpose
Forms Pellets
Generic Name Styrene Butadiene Block Copolymer (SBC)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Automotive Interior Parts
Consumer Applications
General Purpose
Industrial Applications