Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Elastamax™ XL 0117-5 NATURAL Styrene Butadiene Block Copolymer (SBC)

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene-Butadiene Copolymer, SBC
Manufacturer PolyOne Corporation
Trade Name Elastamax™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Elastamax™ XL 0117-5 NATURAL Styrene Butadiene Block Copolymer (SBC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastomers. These materials are ideal for applications requiring flexibility over a wide temperature range, excellent colorability, broad processing capability and durability.A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in accordance with accepted test methods.All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21 for use in the packaging of food. The listings cover many uses and restrictions may apply depending on the application. PLEASE CONTACT US TO REVIEW THE SUITABILITY OF SPECIFIC PRODUCTS IN SPECIFIC APPLICATIONS.This statement is only an overview of the FDA listings for this product. IT IS THE CUSTOMER'S RESPONSIBILITY TO ENSURE THAT THE COMPOUND IS SUITABLE FOR ITS INTENDED APPLICATIONS.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 0.898 g/cc
0.898 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
5 sec; ASTM D2240
Tensile Strength at Break 6.41 MPa
930 psi
510 mm/min; ASTM D412A
Tensile Stress 3.52 MPa

@Strain 300 %
511 psi

@Strain 300 %
510 mm/min; ASTM D412A
Elongation at Break 550 %
550 %
510 mm/min; ASTM D412A
Tear Strength 21.0 kN/m
120 pli
Die C, 510 mm/min; ASTM D624
Compression Set 40 %

@Temperature 70.0 °C,
Time 79200 sec
40 %

@Temperature 158 °F,
Time 22.0 hour
ASTM D395B
Descriptive Properties Value Comments
Agency Ratings FDA Food Contact, Unspecified Rating
Appearance Natural Color
Features Food Contact Acceptable
General Purpose
Forms Pellets
Generic Material SBC
Generic Name Styrene Butadiene Block Copolymer (SBC)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Consumer Applications