PolyOne Elastamax™ XL 0135-33 Styrene Butadiene Block Copolymer (SBC)

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene-Butadiene Copolymer, SBC
Manufacturer PolyOne Corporation
Trade Name Elastamax™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Elastamax™ XL 0135-33 Styrene Butadiene Block Copolymer (SBC).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A thermoplastic elastomer compound formulated for use in food contact applications. The physical properties listed above are typical values obtained on laboratory prepared samples and tested in accordance with accepted test methods.All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21 for use in the packaging of food. The listings cover many uses and restrictions may apply depending on the application. PLEASE CONTACT US TO REVIEW THE SUITABILITY OF SPECIFIC PRODUCTS IN SPECIFIC APPLICATIONS.This statement is only an overview of the FDA listings for this product. IT IS THE CUSTOMER'S RESPONSIBILITY TO ENSURE THAT THE COMPOUND IS SUITABLE FOR ITS INTENDED APPLICATIONS.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 0.898 g/cc
0.898 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.014 cm/cm
0.014 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Shore A 84
84
10 sec; ASTM D2240
Tensile Strength at Break 20.0 MPa
2900 psi
510 mm/min; ASTM D412A
Tensile Stress 5.52 MPa

@Strain 100 %
801 psi

@Strain 100 %
510 mm/min; ASTM D412A
7.58 MPa

@Strain 300 %
1100 psi

@Strain 300 %
510 mm/min; ASTM D412A
Elongation at Break 700 %
700 %
510 mm/min; ASTM D412A
Tear Strength 59.5 kN/m
340 pli
Die C, 510 mm/min; ASTM D624
Descriptive Properties Value Comments
Agency Ratings FDA Food Contact, Unspecified Rating
Appearance Translucent
Features Food Contact Acceptable
General Purpose
Forms Pellets
Generic Material SBC
Generic Name Styrene Butadiene Block Copolymer (SBC)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Consumer Applications
General Purpose
Copyright © lookpolymers.com All Rights Reserved