PolyOne Elastamax™ XL 1088-10 Styrene Butadiene Block Copolymer (SBC) with Mineral Filler  (discontinued **)&l

Category Polymer , Thermoplastic , Styrene-Butadiene , Styrene-Butadiene Copolymer, SBC
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Elastamax™ XL 1088-10 Styrene Butadiene Block Copolymer (SBC) with Mineral Filler  (discontinued **)&l.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc
1.15 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 43

@Time 5.00 sec
43

@Time 0.00139 hour
ASTM D2240
Tensile Strength at Break 3.83 MPa
555 psi
510 mm/min; ASTM D412A
Tensile Strength, Yield 1.21 MPa

@Strain 100 %
175 psi

@Strain 100 %
510 mm/min; ASTM D412A
1.97 MPa

@Strain 300 %
286 psi

@Strain 300 %
510 mm/min; ASTM D412A
Elongation at Break 670 %
670 %
510 mm/min; ASTM D412A
Tear Strength 13.1 kN/m
74.7 pli
Die C, 510 mm/min; ASTM D624
Descriptive Properties Value Comments
Features General Purpose
Forms Pellets
Generic Name Styrene Butadiene Block Copolymer (SBC)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Construction Applications
Consumer Applications
General Purpose
Industrial Applications
Users viewing this material also viewed the following: