Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ 120 Series 121AR Polyvinyl Chloride Homopolymer (PVC Homopolymer)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ 120 Series 121AR Polyvinyl Chloride Homopolymer (PVC Homopolymer).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Note: The value set forth represent typical values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Geon® ALTC and ASTM D638 (formulation): 100phr Geon® 121AR, 57phr DINP, 3phr ESO, and 2phr Therm-Chek SP 120 LOHF Geon® STP 390(formulation): 100phr Geon® 121AR, and 60phr DOPInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Density 0.320 - 0.400 g/cc
0.0116 - 0.0145 lb/in³
ASTM D1505
Fineness 2.5
2.5
North Fineness; Geon® 390
Relative Viscosity 2.71 cP
2.71 cP
Correlation
Brookfield Viscosity 3.0 cP
3.0 cP
Initial, V12, Geon® 1010
4.5 cP
4.5 cP
One Day, V12, Geon® 1010
Viscosity Measurement 1.2
1.2
Inherent; ASTM D1243-60-A
Melt Flow 60 g/10 min

@Pressure 0.655 MPa
60 g/10 min

@Pressure 95.0 psi
Severs Efflux; Geon® 1010
Mechanical Properties Metric English Comments
Tensile Strength 21.0 MPa
3050 psi
Optimum; FF; ASTM D638
Elongation at Yield 400 %
400 %
FF; Optimum Tensile; ASTM D412
Optical Properties Metric English Comments
Gloss 62 %
62 %
60°, FF, ALTC-65
Transmission, Visible 71 %
71 %
FF, ATLC-66
Processing Properties Metric English Comments
Moisture Content 0.070 %
0.070 %
Karl Fisher-Geon® 683
Descriptive Properties Value Comments
Degree of Polymerization 1750
Correlation
Features High Molecular Weight
Forms Powder
Gel Temperature 67 °C
FF, ALTC-29
Generic Material PVC Homopolymer
Generic Name Polyvinyl Chloride Homopolymer (PVC Homopolymer)
K-Value 77
No Standard; Correlation
Methanol Extractables 2.4%
Geon® 894
Polymerization Process Dispersion
Processing Method Dip Coating
Rotational Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America