PolyOne Geon™ Vinyl Flexible 82024 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible 82024 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Automotive OEM approval(s).Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 46
46
15 sec; ASTM D2240
52
52
ASTM D2240
Tensile Strength at Break 7.58 MPa
1100 psi
Type IV, 510 mm/min; ASTM D638
Tensile Strength 2.07 MPa

@Strain 100 %
300 psi

@Strain 100 %
Type IV, 51 mm/min; ASTM D638
Elongation at Break 450 %
450 %
Type IV, 510 mm/min; ASTM D638
Tear Strength 19.3 kN/m
110 pli
Die C, 510 mm/min; ASTM D624
Clash Berg Modulus 0.0138 GPa

@Temperature -35.0 °C
2.00 ksi

@Temperature -31.0 °F
ASTM D1043
0.310 GPa

@Temperature -55.0 °C
45.0 ksi

@Temperature -67.0 °F
ASTM D1043
Thermal Properties Metric English Comments
Brittleness Temperature -60.0 °C
-76.0 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 160 - 168 °C
320 - 334 °F
Descriptive Properties Value Comments
Automotive Specifications CHRYSLER MS-DC225
Features General Purpose
Medium Gloss
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Automotive Applications
General Purpose