PolyOne Geon™ Vinyl Flexible 90453 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible 90453 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Automotive OEM approval(s).Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
15 sec; ASTM D2240
Tensile Strength at Break 16.0 MPa
2320 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 340 %
340 %
Type IV, 510 mm/min; ASTM D638
Tear Strength 75.3 kN/m
430 pli
Die C, 510 mm/min; ASTM D624
Thermal Properties Metric English Comments
Brittleness Temperature -8.00 °C
17.6 °F
ASTM D746
Descriptive Properties Value Comments
Cold Flexibility Pass
GM 9503P; -29°C, 1.91 mm; 25 mm, 4 hr
Features Low Gloss
Fogging 87%
SAE J1756; 6 hrs, 203°F(95°C), 100°F(38°C), after 16 hours
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Automotive Applications
Automotive Interior Trim