Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Packaging 2020 LO-TB Polyvinyl Chloride, Rigid (PVC, Rigid)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Packaging 2020 LO-TB Polyvinyl Chloride, Rigid (PVC, Rigid).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Geon® 2020 LO-TB is a clear blue tint pellet compound designed for water bottle and other low odor appliations that require FDA sanctioned materials.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.31 g/cc
1.31 g/cc
ASTM D792
Density 0.801 g/cc
0.0289 lb/in³
ASTM D1505
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Hardness, Shore D 79
79
ASTM D2240
Tensile Strength, Yield 44.1 MPa
6400 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.32 GPa
336 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 77.2 MPa
11200 psi
ASTM D790
Flexural Modulus 2.64 GPa
383 ksi
ASTM D790
Izod Impact, Notched 11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 62.2 °C

@Thickness 3.18 mm
144 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Optical Properties Metric English Comments
Transmission, Visible 62 %

@Thickness 0.851 mm,
Wavelength 400 nm
62 %

@Thickness 0.0335 in,
Wavelength 400 nm
Internal Method
77 %

@Thickness 0.851 mm,
Wavelength 700 nm
77 %

@Thickness 0.0335 in,
Wavelength 700 nm
Internal Method
Processing Properties Metric English Comments
Mold Temperature 188 - 199 °C
370 - 390 °F
Blow Molding
Descriptive Properties Value Comments
Agency Ratings FDA Food Contact, Unspecified Rating
Appearance Clear/Transparent
Features Food Contact Acceptable
High Gloss
High Impact Resistance
Low to No Odor
Low to No Taste
Forms Pellets
Generic Material PVC, Rigid
Generic Name Polyvinyl Chloride, Rigid (PVC, Rigid)
Processing Method Blow Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Bottles
Packaging