  Online Service   lookpolymers   27660005
Material Notes:
The Cell Classification was determined using the notched Izod test with injection molded samples.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
15 sec; ASTM D2240
Tensile Strength, Yield 40.9 MPa
5930 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.61 GPa
379 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 73.0 MPa
10600 psi
ASTM D790
Flexural Modulus 2.52 GPa
365 ksi
ASTM D790
Izod Impact, Notched 8.10 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
15.2 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Flow; ASTM D256A
11.0 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
20.6 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
Dart Drop Total Energy 36.0 J/cm

@Temperature 23.0 °C
0.0674 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
36.0 J/cm

@Temperature 23.0 °C
0.0674 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 65.0 µm/m-°C
36.1 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 73.9 °C

@Thickness 3.18 mm
165 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 0.749 mm
V-0

@Thickness 0.0295 in
ALL; UL 94
5VA

@Thickness 3.00 mm
5VA

@Thickness 0.118 in
ALL; UL 94
Processing Properties Metric English Comments
Melt Temperature 182 - 193 °C
360 - 379 °F
Descriptive Properties Value Comments
Agency Ratings NSF 51
Ease of Sizing Excellent
Features Good Dimensional Stability
Good Melt Strength
Forms Pellets
Generic Material PVC, Rigid
Generic Name Polyvinyl Chloride, Rigid (PVC, Rigid)
Processing Method Extrusion
PVC Cell Classification 16244
ASTM D1784
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America