PolyOne Geon™ Vinyl Rigid Extrusion 87727-0284 Polyvinyl Chloride, Rigid (PVC, Rigid)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Rigid Extrusion 87727-0284 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Cell Classification was determined using the notched Izod test with injection molded samples. Physical property testing was based on the Geon® 87727 Trans 0020.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 85
85
15 sec; ASTM D2240
Tensile Strength, Yield 56.9 MPa
8250 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 2.87 GPa
416 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 93.5 MPa
13600 psi
ASTM D790
Flexural Modulus 2.92 GPa
424 ksi
ASTM D790
Izod Impact, Notched 0.160 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.300 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Flow; ASTM D256A
0.350 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.656 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Compression Molded, Across Flow; ASTM D256A
2.10 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
3.93 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Dart Drop Total Energy 66.3 J/cm

@Temperature 23.0 °C
0.124 ft-lb/mil

@Temperature 73.4 °F
Procedure A, C.125; ASTM D4226
175 J/cm

@Temperature 23.0 °C
0.328 ft-lb/mil

@Temperature 73.4 °F
Procedure B, C.125; ASTM D4226
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
38.9 µin/in-°F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 61.1 °C

@Thickness 3.18 mm
142 °F

@Thickness 0.125 in
Unannealed; ASTM D648
Flammability, UL94 5VA

@Thickness 1.50 mm
5VA

@Thickness 0.0591 in
TP; UL 94
Processing Properties Metric English Comments
Melt Temperature 182 - 193 °C
360 - 379 °F
Descriptive Properties Value Comments
Appearance Translucent
Forms Pellets
Generic Material PVC, Rigid
Generic Name Polyvinyl Chloride, Rigid (PVC, Rigid)
Processing Method Extrusion
PVC Cell Classification 11553
ASTM D1784
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Capstock
Profiles
Vertical Blinds