PolyOne Geon™ Vinyl Rigid Molding M5000 Polyvinyl Chloride, Rigid (PVC, Rigid)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Rigid Molding M5000 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
ASTM D955
Spiral Flow 58.4 cm
23.0 in
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
ASTM D2240
Tensile Strength, Yield 48.3 MPa
7010 psi
51 mm/min; ASTM D638
Elongation at Break 44 %
44 %
51 mm/min; ASTM D638
Tensile Modulus 2.79 GPa
405 ksi
51 mm/min; ASTM D638
Flexural Strength 75.8 MPa
11000 psi
ASTM D790
Flexural Modulus 2.65 GPa
384 ksi
ASTM D790
Izod Impact, Notched 5.30 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
9.93 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 72.2 °C

@Thickness 6.35 mm
162 °F

@Thickness 0.250 in
Unannealed; ASTM D648
75.0 °C

@Thickness 6.35 mm
167 °F

@Thickness 0.250 in
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 68.9 °C

@Thickness 6.35 mm
156 °F

@Thickness 0.250 in
Unannealed; ASTM D648
72.2 °C

@Thickness 6.35 mm
162 °F

@Thickness 0.250 in
Annealed; ASTM D648
Processing Properties Metric English Comments
Melt Temperature 199 - 210 °C
390 - 410 °F
Descriptive Properties Value Comments
Features General Purpose
Medium Flow
Medium Impact Resistance
Forms Pellets
Generic Material PVC, Rigid
Generic Name Polyvinyl Chloride, Rigid (PVC, Rigid)
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Construction Applications
General Purpose
Outdoor Applications