Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Wire & Cable JC156HN Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Wire & Cable JC156HN Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 84
84
15 sec; ASTM D2240
Tensile Strength, Yield 19.3 MPa
2800 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 380 %
380 %
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -25.0 °C
-13.0 °F
ASTM D746
Oxygen Index 32 %

@Thickness 1.91 mm
32 %

@Thickness 0.0752 in
ASTM D2863
Electrical Properties Metric English Comments
Volume Resistivity 1.30e+14 ohm-cm
1.30e+14 ohm-cm
ASTM D257
Descriptive Properties Value Comments
Additive Lead Stabilizer
Change in Flexural Strength 97%
ASTM D543; 100°C, 1.91 mm; in IRM 902, 4 hr
Change in Ultimate Elongation 54%
ASTM D543; 100°C, 4 hr, in IRM 902 Oil; 0.075 in
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion Coating
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Retention of Tensile Elongation 85%
121°C, 1.91 mm; 336 hr, UL Standard
Retention of Tensile Strength 96%
121°C, 1.91 mm; 336 hr, UL Standard