Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Wire & Cable W1200 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Wire & Cable W1200 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.37 g/cc
1.37 g/cc
ASTM D792
Deformation 25 %

@Temperature 121 °C,
Time 3600 sec
25 %

@Temperature 250 °F,
Time 1.00 hour
500 g; UL 1581
Mechanical Properties Metric English Comments
Hardness, Shore D 41
41
15 sec; ASTM D2240
47
47
ASTM D2240
Tensile Strength, Yield 17.2 MPa
2490 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 250 %
250 %
Type IV, 510 mm/min; ASTM D638
Tensile Modulus 0.0117 GPa
1.70 ksi
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 75.0 °C
167 °F
UL Temperature Rating
80.0 °C
176 °F
UL Temperature Rating
90.0 °C
194 °F
UL Temperature Rating
Brittleness Temperature -5.00 °C
23.0 °F
ASTM D746
Electrical Properties Metric English Comments
Volume Resistivity 1.50e+12 ohm-cm
1.50e+12 ohm-cm
ASTM D257
Dissipation Factor 0.090

@Frequency 1000 Hz,
Temperature 30.0 °C
0.090

@Frequency 1000 Hz,
Temperature 86.0 °F
24 hr; ASTM D150
Processing Properties Metric English Comments
Melt Temperature 188 - 193 °C
370 - 379 °F
Descriptive Properties Value Comments
Additive Lead Stabilizer
Agency Ratings UL QMTT2
Appearance Black
Dark Grey
Change in Ultimate Elongation 25%
ASTM D543; 60°C, 1440 hr, in ASTM #2 Oil; 0.075 in
Features Flame Retardant
Sunlight Resistant (300 hours)
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Extrusion Coating
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Retention of Tensile Elongation 70%
113°C, 1.91 mm; 168 hr, UL Standard
90%
100°C, 1.91 mm; 168 hr, UL Standard
Uses Building Wire Insulation
Wire & Cable Applications
Wire Types AWM
THW