Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Wire & Cable WJCK502L Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Wire and Cable Grade
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Wire & Cable WJCK502L Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Typical Properties of Molded Slab (0.075); Not to be Construed as Specifications. Provisional Product Information - Physical and Mechanical properties based on initial production.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 78
78
15 sec; ASTM D2240
Tensile Strength, Yield 13.1 MPa
1900 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 300 %
300 %
Type IV, 510 mm/min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -46.0 °C
-50.8 °F
ASTM D746
Oxygen Index 25 %

@Thickness 1.91 mm
25 %

@Thickness 0.0752 in
ASTM D2863
Processing Properties Metric English Comments
Melt Temperature 160 - 170 °C
320 - 338 °F
Descriptive Properties Value Comments
Agency Ratings CSA LAG (Low Acid Gas)
CSA Unspecified Rating
Features Flame Retardant
Good UV Resistance
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
HCL Evolution 13%
CSA C22.2 No. 0.3
Processing Method Extrusion Coating
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Retention of Tensile Elongation 85%
121°C, 889.0 µm; 336 hr, UL Standard
Retention of Tensile Strength 110%
121°C, 889.0 µm; 336 hr, UL Standard
RoHS Compliance RoHS Compliant
Uses Cable Jacketing
Wire & Cable Applications