PolyOne Geon® XV3811B Thermoplastic Elastomer - PVC/TPU  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Vinyl (PVC)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon® XV3811B Thermoplastic Elastomer - PVC/TPU  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications:Hose and TubingCustom ProfilesProcessing Method:Extrusion and MoldingExtrusion-ProfileInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 68
68
15 sec; ASTM D2240
Tensile Strength, Ultimate 18.44 MPa
2675 psi
Type 4 - Flexibles, 20 in/min; ASTM D638
Elongation at Break 375 %
375 %
Type 4 - Flexibles, 20 in/min; ASTM D638
Thermal Properties Metric English Comments
Brittleness Temperature -43.9 °C
-47.0 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 171 - 177 °C
340 - 350 °F
Extrusion
188 - 199 °C
370 - 390 °F
Molding
Descriptive Properties Value Comments
Product Form Pellets