PolyOne Lubri-Tech™ SF-25GF/13T-2S Polyphenylene Sulfide (PPS), Glass Filled, PTFE/Silicone Lubricated  (disco

Category Polymer , Thermoplastic , Polyphenylene Sulfide (PPS)
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Lubri-Tech™ SF-25GF/13T-2S Polyphenylene Sulfide (PPS), Glass Filled, PTFE/Silicone Lubricated  (disco.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Glass Fiber ReinforcedPTFE/Silicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.61 g/cc
1.61 g/cc
ASTM D792
Linear Mold Shrinkage 0.0025 - 0.0030 cm/cm
0.0025 - 0.0030 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 124 MPa
18000 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 8.27 GPa
1200 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 179 MPa
26000 psi
ASTM D790
Flexural Modulus 8.27 GPa
1200 ksi
ASTM D790
Izod Impact, Notched 0.854 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.60 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Processing Properties Metric English Comments
Melt Temperature 299 - 332 °C
570 - 630 °F
Molding
Mold Temperature 135 - 149 °C
275 - 300 °F
Drying Temperature 135 - 149 °C
275 - 300 °F
Dry Time 2 hour
2 hour
Descriptive Properties Value Comments
Product Form Pellets