Material Notes:
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. LubriOne compounds have been demonstrated to reduce friction, noise, vibration, heat buildup and improve product durability.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.70 g/cc
1.70 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0025 cm/cm
0.0020 - 0.0025 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 138 MPa
20000 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 4.0 %
4.0 %
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 12.1 GPa
1750 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 159 MPa
23100 psi
ASTM D790
Flexural Modulus 10.3 GPa
1490 ksi
ASTM D790
Izod Impact, Notched 1.10 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
2.06 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 270 °C
518 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
Unannealed; ASTM D648
Flammability, UL94 V-0
V-0
UL 94
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+14 ohm-cm
1.00e+14 ohm-cm
ASTM D257
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
ASTM D257
Processing Properties Metric English Comments
Mold Temperature 130 - 150 °C
266 - 302 °F
Drying Temperature 140 - 150 °C
284 - 302 °F
Dry Time 4.00 hour
4.00 hour
Descriptive Properties Value Comments
Features Lubricated
Forms Pellets
Generic Material PPS
Generic Name Polyphenylene Sulfide (PPS)
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Uses Appliance Components
Conveyor Parts
Printer Parts