Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Maxxam™ FR PE126 BLK 3330 Polyethylene, Low Density (LDPE)

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE
Manufacturer PolyOne Corporation
Trade Name Maxxam™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Maxxam™ FR PE126 BLK 3330 Polyethylene, Low Density (LDPE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V-0, and 5VA performance ratings. In addition, many compounds in the Maxxam FR portfolio offer elevated Relative Thermal Index (RTI) ratings.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 0.998 g/cc
0.998 g/cc
ASTM D792
Melt Flow 0.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Procedure A; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 15.9 MPa
2310 psi
Type I, 51 mm/min; ASTM D638
Elongation at Break 140 %
140 %
Type I, 51 mm/min; ASTM D638
Thermal Properties Metric English Comments
Flammability, UL94 V-2

@Thickness 1.59 mm
V-2

@Thickness 0.0626 in
Internal Method
Descriptive Properties Value Comments
Appearance Black
Features Flame Retardant
Forms Pellets
Generic Material LDPE
Generic Name Polyethylene, Low Density (LDPE)
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Users viewing this material also viewed the following: