Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Maxxam™ FR PO Conc 62 Polypropylene, Unspecified (PP, Unspecified)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer PolyOne Corporation
Trade Name Maxxam™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Maxxam™ FR PO Conc 62 Polypropylene, Unspecified (PP, Unspecified).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V-0, and 5VA performance ratings. In addition, many compounds in the Maxxam FR portfolio offer elevated Relative Thermal Index (RTI) ratings.MAXXAM FR PO Concentrate 62 is designated to impart good flame retardancy and UV stbility to low and high density polyethylene. Because there are so many varieties of polyethylene, it is difficult to predict the let-down ratio required to meet the specific flammability standards. For starting point formulations we would suggest:4-7 parts by weight of Low Density Polyethylene-,5 parts by weight of High Density Polyethylene-to 1 part of Concentrate 62. When this concentrate is letdown at the proper ratio the resulting materials can achieve flame retardancy equivalent to the requirements of the UL-94 V-2 or VTM-2. BFD IX-1 and NFPA 701 preformance criteria achievable using 8% PO CONC 62 in LDPE film @ 4-8 mil film / V-2 preformance criteria achievable in PE @ 15-30% in thickness >/= 1.5mm. The effects on the physicals should be minimal.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.67 g/cc
1.67 g/cc
ASTM D792
Melt Flow 2.7 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.7 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Procedure A; ASTM D1238
Descriptive Properties Value Comments
Features Flame Retardant
Forms Pellets
Generic Material PP, Unspecified
Generic Name Polypropylene, Unspecified (PP, Unspecified)
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Users viewing this material also viewed the following: