Material Notes:
Maxxam™ HFFR WC-P85 RoHS Natural is a halogen-free flame retardant polyolefin compound characterized by low smoke, low flame spread, excellent spring-back, no plate-out and high extrusion line speed. It is designed for very thin-wall (0.5 mm or 20 mills), flexible, primary conduit applications for optical fiber cables among others. It is also excellent for injection molding.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Melt Flow 7.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
7.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 43
43
10 sec; ASTM D2240
48
48
ASTM D2240
Tensile Strength at Break 8.96 MPa
1300 psi
51 mm/min; ASTM D638
Elongation at Break 450 %
450 %
51 mm/min; ASTM D638
Flexural Modulus 0.296 GPa
42.9 ksi
13 mm/min; ASTM D790
Thermal Properties Metric English Comments
Flammability, UL94 V-0

@Thickness 1.55 mm
V-0

@Thickness 0.0610 in
molded specimen; UL 94
Oxygen Index >= 33 %
>= 33 %
ASTM D2863
Descriptive Properties Value Comments
Features Flame Retardant
Good Chemical Resistance
Good Colorability
Good Processability
Halogen Free
Low Smoke Emission
Low Toxicity
Forms Pellets
Generic Material Polyolefin, Unspecified
Generic Name Polyolefin, Unspecified
Processing Method Extrusion
Injection Molding
Regional Availability North America
RoHS Compliance RoHS Compliant
Uses Conduit
Corrugated Pipe
Wire & Cable Applications