PolyOne Maxxam™ MAXBATCH YM-618.G001-1000 Polypropylene, Unspecified (PP, Unspecified)

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer PolyOne Corporation
Trade Name Maxxam™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Maxxam™ MAXBATCH YM-618.G001-1000 Polypropylene, Unspecified (PP, Unspecified).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium carbonate, glass and talc to provide a desired balance of properties including stiffness, durability, impact resistance and heat resistance. Custom grades are available with features such as UV stabilizers, heat stabilizers, custom color, high impact, etc.MAXBATCH PRODUCTS ARE DESIGNED TO BE USED AS A LETDOWN WITH ADDITIONAL POLYPROPYLENE.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.70 g/cc
1.70 g/cc
ASTM D792
Melt Flow 1.8 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.8 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Procedure A; ASTM D1238
Descriptive Properties Value Comments
Appearance Natural Color
Features General Purpose
Filler / Reinforcement Talc Filler
Unspecified FillerReinfor., 70% Filler by Weight
Forms Pellets
Generic Material PP, Unspecified
Generic Name Polypropylene, Unspecified (PP, Unspecified)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Automotive Applications
Construction Applications
Consumer Applications
General Purpose
Industrial Applications