Material Notes:
Maxxam ™ SY 89-21-1 is a polypropylene copolymer compound with a pre-dispersed blowing agent for up to 50% expansion. The compound offers consistent cell structure, dielectric properties, and strength on insulation walls as thin as 10 mils.NOTE: 1. Typical properties of molded slab (0.075); Not to be construedas specifications.2. Foam density reduction depends upon loading level, temperatureand residence time before cooling.3. Recommended process temperature: 190°C to 220°C (375°F to430°F).Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 0.579 g/cc
0.579 g/cc
ASTM D792
Melt Flow 2.1 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.1 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Procedure A; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.4 MPa
3390 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 400 %
400 %
Type IV, 510 mm/min; ASTM D638
Electrical Properties Metric English Comments
Dielectric Constant 2.24

@Frequency 1000 Hz
2.24

@Frequency 1000 Hz
ASTM D150
Dissipation Factor 0.00030

@Frequency 1000 Hz
0.00030

@Frequency 1000 Hz
ASTM D150
Descriptive Properties Value Comments
Features Foamable
Forms Pellets
Generic Material PP, Unspecified
Generic Name Polypropylene, Unspecified (PP, Unspecified)
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Cable Jacketing
Communication Wire Insulation
Wire & Cable Applications
Copyright © lookpolymers.com All Rights Reserved