PolyOne Novablend™ 2677 Polyvinyl Chloride, Rigid (PVC, Rigid)

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer PolyOne Corporation
Trade Name Novablend™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Novablend™ 2677 Polyvinyl Chloride, Rigid (PVC, Rigid).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.36 g/cc
1.36 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 51.7 MPa
7500 psi
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 3.10 GPa
450 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 82.7 MPa
12000 psi
ASTM D790
Flexural Modulus 2.76 GPa
400 ksi
ASTM D790
Izod Impact, Notched 0.640 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
1.20 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 66.7 °C

@Thickness 1.57 mm
152 °F

@Thickness 0.0618 in
Annealed; ASTM D648
Descriptive Properties Value Comments
Appearance Clear/Transparent
Features Excellent Printability
Good UV Resistance
High Gloss
Forms Pellets
Generic Material PVC, Rigid
Generic Name Polyvinyl Chloride, Rigid (PVC, Rigid)
Regional Availability North America
Uses Film
General Purpose