PolyOne OnFlex™ BIO 5170D-E0010 Thermoplastic Elastomer (TPE)

Category Polymer , Renewable/Recycled Polymer , Thermoplastic , Elastomer, TPE
Manufacturer PolyOne Corporation
Trade Name OnFlex™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne OnFlex™ BIO 5170D-E0010 Thermoplastic Elastomer (TPE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
OnFlex™ BIO 5100 series thermoplastic elastomer compounds are glass reinforced thermoplastic polyurethane compounds made from renewable natural sources. These compounds contain at least 20% renewable material as certified according to ASTM-D6866. The OnFlex™ BIO 5100 series compounds are formulated to provide excellent toughness, abrasion resistance and mechanical properties.Properties are measured using injection molded plaques.Information provided by PolyOne
Physical Properties Metric English Comments
Density 1.34 g/cc
0.0484 lb/in³
ISO 1183
Filler Content 20 %
20 %
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
ISO 868
Tensile Strength at Break 65.0 MPa
9430 psi
ISO 527-2
Elongation at Break 15 %
15 %
ISO 527-2
Tensile Modulus 1.20 GPa
174 ksi
ISO 527-2
Flexural Strength 40.0 MPa
5800 psi
ISO 178
Flexural Modulus 1.10 GPa
160 ksi
ISO 178
Charpy Impact Unnotched 3.00 J/cm²

@Temperature -30.0 °C
14.3 ft-lb/in²

@Temperature -22.0 °F
ISO 179
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179
Charpy Impact, Notched 0.600 J/cm²

@Temperature -30.0 °C
2.86 ft-lb/in²

@Temperature -22.0 °F
ISO 179
3.50 J/cm²

@Temperature 23.0 °C
16.7 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Processing Properties Metric English Comments
Melt Temperature 225 - 250 °C
437 - 482 °F
Mold Temperature 30.0 - 60.0 °C
86.0 - 140 °F
Drying Temperature 100 - 120 °C
212 - 248 °F
Dry Time 1.00 - 2.00 hour
1.00 - 2.00 hour
Descriptive Properties Value Comments
Biobased Content 34%
ASTM D6866
Features Good Abrasion Resistance
Good Toughness
Renewable Resource Content
Forms Pellets
Generic Material TPE
Generic Name Thermoplastic Elastomer (TPE)
Injection Rate Slow
Manufacturer / Supplier GLS Thermoplastic Elastomers
Processing Method Injection Molding
Multi Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Uses Automotive Applications
Consumer Applications
General Purpose
Sporting Goods