PolyOne Stat-Tech™ CTX-20SS 107/000 Keytec Blue Polyamide 6/12 Copolymer (Nylon 6/12)

Category Polymer , Thermoplastic , Nylon , Nylon 612
Manufacturer PolyOne Corporation
Trade Name Stat-Tech™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Stat-Tech™ CTX-20SS 107/000 Keytec Blue Polyamide 6/12 Copolymer (Nylon 6/12).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compounds combine the performance of select engineering resins with reinforcing additives such as carbon powder, carbon fiber, nickel-coated carbon fiber and stainless steel fiber, for low to high levels of conductivity depending upon application requirements.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.32 g/cc
1.32 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.015 - 0.016 cm/cm
0.015 - 0.016 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.012 - 0.013 cm/cm
0.012 - 0.013 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 54.1 MPa
7850 psi
ASTM D638
Elongation at Break 39 %
39 %
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 85.8 MPa
12400 psi
ASTM D790
Flexural Modulus 2.74 GPa
397 ksi
ASTM D790
Izod Impact, Notched 0.520 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.974 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) >= 245 °C
>= 473 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity <= 1.00e+12 ohm-cm
<= 1.00e+12 ohm-cm
ASTM D257
Surface Resistance <= 1.00e+12 ohm
<= 1.00e+12 ohm
ASTM D257
Static Decay 0.40 sec
0.40 sec
(Mil-B-81705C), 12% RH, 5000kV to 50kV
Shielding Effectiveness 5.0 dB

@Frequency 1.00e+10 Hz
5.0 dB

@Frequency 1.00e+10 Hz
1/8 thickness
10 dB

@Frequency 5.00e+9 Hz
10 dB

@Frequency 5.00e+9 Hz
1/8 thickness
Descriptive Properties Value Comments
Features Electromagnetic Shielding (EMI)
Filler / Reinforcement Stainless Steel Fiber
Forms Pellets
Generic Material Nylon 6/12
Generic Name Polyamide 6/12 Copolymer (Nylon 6/12)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Aerospace Applications
Automotive Electronics
Computer Components
Connectors
Electrical Housing
Electrical/Electronic Applications
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved