PolyOne Synprene® RT-3730 Thermoplastic Elastomer - SBC, Mineral Filled  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Synprene® RT-3730 Thermoplastic Elastomer - SBC, Mineral Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledNaturalApplications:General PurposeMarket:Consumer GoodsIndustrialBuilding and ConstructionProcessing Method:Injection MoldingPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.12 g/cc
1.12 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 32
32
Instant; ASTM D2240
Tensile Strength, Yield 3.45 MPa
500 psi
Method A (Dumbbell & Section), 20 in/min, Break; ASTM D412
0.896 MPa

@Strain 300 %
130 psi

@Strain 300 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Elongation at Break 850 %
850 %
Method A (Dumbbell & Section), 20 in/min; ASTM D412
Rebound 40 %
40 %
Bayshore; ASTM D2632
Tear Strength 11.7 kN/m
67.0 pli
Die C (graves), 20 in/min; ASTM D624
Compression Set 15 %
15 %
Method B, 73°F(23°C), 22 hrs; ASTM D395