Material Notes:
Description/Features:Thermally ConductiveCeramic FilledPolyOne First ChoiceInformation provided by PolyOne Corporation.
Physical Properties Metric English Comments
Specific Gravity 1.68 g/cc
1.68 g/cc
ASTM D792
Water Absorption 0.10 %

@Thickness 0.508 mm
0.10 %

@Thickness 0.0200 in
24 hr. Immersion; ASTM D570
Linear Mold Shrinkage 0.0039 cm/cm
0.0039 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 56.5 MPa
8190 psi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Elongation at Break 0.45 %
0.45 %
Type 1 - Rigids, 0.2 in/min; ASTM D638
Tensile Modulus 26.3 GPa
3810 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
Flexural Strength 81.43 MPa
11810 psi
ASTM D790
Flexural Modulus 15.0 GPa
2180 ksi
ASTM D790
Poissons Ratio 0.24
0.24
ASTM E132
Shear Modulus 10.6 GPa
1540 ksi
Calculated
Izod Impact, Notched 0.214 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
0.400 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Method A, Injection Molded; ASTM D256
Thermal Properties Metric English Comments
Thermal Conductivity >= 5.99 W/m-K
>= 41.6 BTU-in/hr-ft²-°F
ASTM C177
Deflection Temperature at 1.8 MPa (264 psi) 196 °C
385 °F
Annealed, 0.125 in bars; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 6.6 ohm-cm
6.6 ohm-cm
ASTM D257
Dielectric Constant 3.46

@Frequency 1e+6 Hz
3.46

@Frequency 1e+6 Hz
ASTM D150
Descriptive Properties Value Comments
Product Form Pellets