Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Trilliant™ HC HC9820-0030 RS Natural Polyetheretherketone (PEEK)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer PolyOne Corporation
Trade Name Trilliant™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Trilliant™ HC HC9820-0030 RS Natural Polyetheretherketone (PEEK).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead of the competition. When specified, Trilliant® compounds may incorporate agency rated materials that meet USP Class VI, FDA or ISO 10993 testing requirements.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.51 g/cc
1.51 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.011 cm/cm
0.011 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 177 MPa
25700 psi
Type I, 51 mm/min; ASTM D638
Elongation at Break 9.0 %
9.0 %
Type I, 51 mm/min; ASTM D638
Flexural Strength 259 MPa
37600 psi
ASTM D790
Flexural Modulus 8.96 GPa
1300 ksi
ASTM D790
Izod Impact, Notched 1.20 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
2.25 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Melting Point 360 - 382 °C
680 - 720 °F
Deflection Temperature at 0.46 MPa (66 psi) >= 245 °C

@Thickness 3.18 mm
>= 473 °F

@Thickness 0.125 in
Annealed; ASTM D648
Processing Properties Metric English Comments
Mold Temperature 163 - 177 °C
325 - 351 °F
Drying Temperature 104 °C
219 °F
Dry Time 3.00 hour
3.00 hour
Descriptive Properties Value Comments
Agency Ratings USP Class VI
Appearance Natural Color
Features Biocompatible
Good Chemical Resistance
Medium Impact Resistance
Specialty Grade
Filler / Reinforcement Glass Fiber Reinforcement, 30% Filler by Weight
Forms Pellets
Generic Material PEEK
Generic Name Polyetheretherketone (PEEK)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses High Temperature Applications
Hospital Goods
Medical/Healthcare Applications
Copyright © lookpolymers.com All Rights Reserved