Material Notes:
AKRYLON XT sheets have good optical properties and high quality surfaces. AKRYLON XT sheets also show excellent color and functional stability and can be used in contact with foodstuffs. AKRYLON XT sheets also combine the following excellent properties: brilliant transparency, very good weathering and ageing resistance, high surface stability/resistance, and good recyclability.Construction components Light domes Partition walls Glazing Roofing Windows for caravans Lighting Prismatic control lenses Opal diffusers Engineering components Housings Machine Covers Advertising and Decorations Letters Decorations Shop fittings Advertising panels Point of Purchase DisplaysQuinn Manufacturing Group rebranded its Plastics Division as Polycasa in 2013.
Physical Properties Metric English Comments
Density 1.19 g/cc
0.0430 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Ball Indentation Hardness 175 MPa
25400 psi
ISO 2039-1
Tensile Strength at Break 70.0 MPa
10200 psi
ISO 527-2
Elongation at Break 4.0 %
4.0 %
ISO 527-2
Tensile Modulus 3.20 GPa
464 ksi
ISO 527-2
Flexural Strength 115 MPa
16700 psi
ISO 178
Charpy Impact Unnotched 1.70 J/cm²
8.09 ft-lb/in²
ISO 179
Charpy Impact, Notched 0.200 J/cm²
0.952 ft-lb/in²
ISO 179
Thermal Properties Metric English Comments
CTE, linear 70.0 µm/m-°C

@Temperature 20.0 °C
38.9 µin/in-°F

@Temperature 68.0 °F
DIN 53752
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C
203 °F
ISO 75
Vicat Softening Point 105 °C
221 °F
ISO 306
Decomposition Temperature >= 280 °C
>= 536 °F
Optical Properties Metric English Comments
Refractive Index 1.492
1.492
ISO 489
Haze 0.60 %
0.60 %
AKRYLON XT clear; ISO 14782
Transmission, Visible 93 %

@Thickness 3.00 mm
93 %

@Thickness 0.118 in
ISO 1183
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+15 - 5.00e+15 ohm-cm
1.00e+15 - 5.00e+15 ohm-cm
IEC 60093
Surface Resistance 3.00e+15 - 3.00e+16 ohm
3.00e+15 - 3.00e+16 ohm
IEC 60093
Dielectric Constant 2.7

@Frequency 1e+6 Hz
2.7

@Frequency 1e+6 Hz
2.7

@Frequency 50 Hz
2.7

@Frequency 50 Hz
3.1

@Frequency 1000 Hz
3.1

@Frequency 1000 Hz
Dielectric Strength 30.0 kV/mm

@Thickness 1.00 mm
762 kV/in

@Thickness 0.0394 in
DIN 53481
Descriptive Properties Value Comments
Combustibility Grade E
EN 13501-1
Electrical Strength, kV/mm² 10
IEC 60243-1
Users viewing this material also viewed the following: