Material Notes:
Good ink adhesionGood receptabilityStable sheet dimensionsHigh impact strengthGood chemical resistanceEnvironmentally safeRecyclableMeets current food contact legislationDisplays Graphic Arts Advertising Packaging Invitations Business cards Covers for CD, Video, books Toys Promotional gifts Book marks Post cards Mouse pads Puzzles Buttons Light switch plates Wrist bands Masks StickersQuinn Manufacturing Group rebranded its Plastics Division as Polycasa in 2013.
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength at Break 50.0 MPa
7250 psi
ISO 527-2
Elongation at Break 54 %
54 %
ISO 527-2
Tensile Modulus 2.20 GPa
319 ksi
ISO 527-2
Flexural Strength 70.0 MPa
10200 psi
ISO 178
Flexural Modulus 2.075 GPa
301.0 ksi
ISO 178
Charpy Impact Unnotched NB
NB
ISO 179
Charpy Impact, Notched 1.00 J/cm²
4.76 ft-lb/in²
ISO 179-1
Thermal Properties Metric English Comments
CTE, linear 68.0 µm/m-°C

@Temperature 20.0 °C
37.8 µin/in-°F

@Temperature 68.0 °F
DIN 53752
Specific Heat Capacity 1.10 J/g-°C
0.263 BTU/lb-°F
IES 1006
Thermal Conductivity 0.200 W/m-K
1.39 BTU-in/hr-ft²-°F
DIN 52612
Maximum Service Temperature, Air 70.0 °C
158 °F
Deflection Temperature at 0.46 MPa (66 psi) 72.0 °C
162 °F
ISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 68.0 °C
154 °F
ISO 75-2
Vicat Softening Point 82.0 °C
180 °F
ISO 306
Decomposition Temperature >= 280 °C
>= 536 °F
Optical Properties Metric English Comments
Refractive Index 1.57
1.57
ISO 489
Haze <= 1.0 %
<= 1.0 %
ASTM D1003
Transmission, Visible 88 %
88 %
DIN 5036
Electrical Properties Metric English Comments
Volume Resistivity 6.05e+14 ohm-cm
6.05e+14 ohm-cm
IEC 93
Surface Resistance 6.62e+14 ohm
6.62e+14 ohm
IEC 93
Dielectric Constant 2.6

@Frequency 1000 Hz
2.6

@Frequency 1000 Hz
IEC 250
Dielectric Strength 10.7 kV/mm
272 kV/in
IEC 60243-1
Dissipation Factor 0.010

@Frequency 50 Hz
0.010

@Frequency 50 Hz
IEC 250
Processing Properties Metric English Comments
Processing Temperature 120 - 160 °C
248 - 320 °F
Sheet Forming