Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polykemi AB POLYelast TPE ZSB60650 Thermoplastic Elastomer, SEBS/SBS-based, Mineral Reinforced

Category Polymer , Thermoplastic , Elastomer, TPE , Styrene-Butadiene , Styrene/Butadiene/Styrene (SBS)
Manufacturer Polykemi AB
Trade Name POLYelast
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB POLYelast TPE ZSB60650 Thermoplastic Elastomer, SEBS/SBS-based, Mineral Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.30 g/cc
0.0470 lb/in³
ISO 1183
Melt Index of Compound 10 g/10 min

@Load 5.00 kg,
Temperature 190 °C
10 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 74

@Time 15.0 sec
74

@Time 0.00417 hour
Polykemi
Tensile Strength at Break <= 5.50 MPa
<= 798 psi
ISO/R527
Elongation at Break 670 %
670 %
ISO/R527
100% Modulus 0.00300 GPa
0.435 ksi
ISO/R527
300% Modulus 0.00400 GPa
0.580 ksi
ISO/R527
Compression Set 42.8 %

@Temperature 23.0 °C,
Time 259000 sec
42.8 %

@Temperature 73.4 °F,
Time 72.0 hour
DIN 53517
88.3 %

@Temperature 70.0 °C,
Time 86400 sec
88.3 %

@Temperature 158 °F,
Time 24.0 hour
DIN 53517
Processing Properties Metric English Comments
Melt Temperature 180 - 220 °C
356 - 428 °F
Mold Temperature 20.0 - 40.0 °C
68.0 - 104 °F
Back Pressure 0.500 - 1.50 MPa
72.5 - 218 psi
Descriptive Properties Value Comments
Holding Pressure () Low
% of injection pressure
Injection Pressure Low
Injection Speed () High