Polykemi AB POLYshine PBT D611 PBT

Category Polymer , Thermoplastic , Polyester, TP , Polybutylene Terephthalate (PBT)
Manufacturer Polykemi AB
Trade Name POLYshine
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polykemi AB POLYshine PBT D611 PBT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Polykemi AB
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
ISO 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break <= 45.0 MPa
<= 6530 psi
ISO/R527
Elongation at Break 365 %
365 %
ISO/R527
Flexural Strength <= 66.0 MPa
<= 9570 psi
ISO 178
Flexural Modulus 1.90 GPa

@Temperature 23.0 °C
276 ksi

@Temperature 73.4 °F
ISO 178
Charpy Impact, Notched 1.00 J/cm²

@Temperature -20.0 °C
4.76 ft-lb/in²

@Temperature -4.00 °F
ISO 179
1.70 J/cm²

@Temperature 23.0 °C
8.09 ft-lb/in²

@Temperature 73.4 °F
ISO 179
Thermal Properties Metric English Comments
Vicat Softening Point 161 °C

@Load 5.001 kg
322 °F

@Load 11.03 lb
50°C/h; ISO 306
218 °C

@Load 1.00 kg
424 °F

@Load 2.21 lb
50°C/h; ISO 306