Material Notes:
Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processingTypical Applications: IndustrialPackagingConsumerHeathcareInformation from Alliance Polymers & Services, Distributor of Nantong Elastomer Technology Co.Ltd
Physical Properties Metric English Comments
Specific Gravity 1.01 g/cc
1.01 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 95
95
ASTM D2240
Tensile Stress 10.1 MPa

@Strain 100 %
1460 psi

@Strain 100 %
ASTM D412
11.8 MPa

@Strain 300 %
1710 psi

@Strain 300 %
ASTM D412
Tensile Strength, Yield 14.6 MPa
2120 psi
ASTM D412
Elongation at Break 510 %
510 %
ASTM D412