Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Industries Densetec HDPE Cutting Board

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Injection Molded
Manufacturer Polymer Industries
Trade Name Densetec
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polymer Industries Densetec HDPE Cutting Board.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Densetec Cutting Board is engineered for durability, low maintenance and safety. Its textured, matte surface safely holds food in place without slipping. The "natural" bright white color is favored for its sanitary look. Knives stay sharp when cutting on Densetec Cutting Board. Instead of striking a rigid surface that dulls the blade, Densetec Cutting Board gives on contact. Because of its unique molecular structure, cuts seal and become indiscernible.Information provided by Polymer Industries.
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM D1505
ESCR 100% Igepal® 35 hour
35 hour
CO-630; Condition B; ASTM D1693
45 hour
45 hour
CO-630; Condition A; ASTM D1693
Melt Index of Compound 0.25 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.25 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
2in (50mm) per min.; ASTM D638 Type 4
Elongation at Break >= 600 %
>= 600 %
2in (50mm) per min.; ASTM D638 Type 4
Flexural Modulus 1.378 GPa
199.9 ksi
ASTM D790
Thermal Properties Metric English Comments
CTE, linear 126 µm/m-°C

@Temperature 20.0 °C
70.0 µin/in-°F

@Temperature 68.0 °F
ASTM E831
Brittleness Temperature <= -84.0 °C
<= -119 °F
ASTM D746
Flammability, UL94 HB
HB
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved