Material Notes:
The material displays improved performance characteristics in a variety of piping applications. In addition the material is UV stabilized and ideal for use in demanding outdoor applications. It retains its properties between 220°F and 180°F, and resists most chemicals. It is also NSF certified under Standard 61 to be used in potable water piping systems.Information provided by Polymer Industries.
Physical Properties Metric English Comments
Density 0.944 g/cc
0.0341 lb/in³
ASTM D1505
High Load Melt Index 11 g/10 min

@Load 21.6 kg,
Temperature 190 °C
11 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
PENT >= 100 hour
>= 100 hour
Slow Crack Growth; ASTM F1473
Tensile Strength, Yield 22.0 MPa
3190 psi
2in (50mm) per min.; ASTM D638 Type 4
Elongation at Break 800 %
800 %
2in (50mm) per min.; ASTM D638 Type 4
Flexural Modulus 0.760 GPa
110 ksi
2% Secant; ASTM D3350
0.960 GPa
139 ksi
Tangent; ASTM D790
Hydrostatic Design Basis 5.50 MPa
798 psi
140°F; ASTM D2837
11.0 MPa

@Temperature 23.0 °C
1600 psi

@Temperature 73.4 °F
ASTM D2837
Thermal Properties Metric English Comments
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746